Old 10-03-2009, 07:24 PM   #1
New Member
 
2010 30' Classic
1975 28' Argosy 28
Eleele , Hawaii
Join Date: Oct 2009
Posts: 2
Repairing galvanic corrosion holes

I have been researching "aluminum body panel repair" on the internet and stumbled across this site. I am hoping someone can tell me the proper way to repair holes caused by galvanic corrosion (which will be painted). What I have learned so far is:

1. Drill;, rasp; or otherwise (but do not grind) to remove the aluminum which has oxidized to a white powder all around the perimeter until the hole has a 'solid' aluminum edge.

2. Prime the cleaned hole w/ a zinc chromate primer.

From this point forward I have several choices:

3 a. Cover the cleaned and primed hole with 3M aluminum autobody repair tape and spread, sand, and feather a plastic (or aluminum powder based) autobody filler in successive layers; or b. Spread a layer of autobody filler, imbed a piece of aluminum or fiberglass screen and squeege flat. After the filler has cured, rough sand w/ #80 paper to a level surface at the edges. Successive layers of filler can be added and sanded until the entire surface is level and feathered into the surrounding area.

4. Final sand the patch with #320 wet paper to remove any scratches; prime with a sandable automotive primer; lightly dry sand with #320, blow off dust; clean the area with an automotive refinishing degreaser; and tack rag the surface to remove any stray dust particles before applying the finish coat(s).

Any first-hand recommendations as to proceedures, materials, etc. are greatly appreciated.
Panaman is offline   Reply With Quote
Old 10-03-2009, 08:20 PM   #2
Rivet Master

 
1972 25' Tradewind
Currently Looking...
McHenry County , Illinois
Join Date: Jul 2003
Posts: 1,171
Images: 5
The first question. What is the application? Is this a structural or cosmetic repair?
This is important because if you’re to fill a perforated piece of sheet metal, especially aluminum, with "bondo" it will fail in a short period of time.
If the patch is big enough to require a backing tape dam and screen reinforcement I would be inclined to replace the panel or MIG weld in an aluminum patch.
If the holes are only about an inch or so, and it’s cosmetic, I might be inclined to try one of the 3M Automix Epoxies. After sanding down to the surface and priming, do a final fill with spot putty.
Find a jobber to help you find the right mix for your application because the 3M catalog is huge. Currently they are changing all the product numbers and deleting obsolete items. Our guy seems to always have to call in for the current number.

Tom
__________________

Tom Nugler is offline   Reply With Quote
Old 10-04-2009, 10:33 AM   #3
New Member
 
2010 30' Classic
1975 28' Argosy 28
Eleele , Hawaii
Join Date: Oct 2009
Posts: 2
Thanks to Tom for his suggestions above.

I will clarify the issue by saying that the perforations are not structural, only small (+/- 1/2") and cosmetic. The back of the panels in question are not easily accessible which is why I thought using a screen or aluminum tape 'backer' to be advisable so as to give the filler something to 'bite' to over the perforation.

Just an additional note for others: Thoroughly clean all tools which may have been previously used on steel or other metals as using such tools w/o cleaning greatly increases the risk of further cross contamination of the aluminum which is the cause of this type of corrosion in the first place. It only takes a microscopic particle of steel in direct contact with an aluminum panel to start such corrosive action.

Panaman
Panaman is offline   Reply With Quote
Reply


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Galvanic Reaction Help Ganglin Ribs, Skins & Rivets 16 09-12-2009 10:21 PM
Galvanic corrosion question reggiemon Ribs, Skins & Rivets 4 04-11-2009 05:01 PM
New toilet holes don't match old holes RichHog Sinks, Showers & Toilets 8 03-15-2009 06:36 PM
Corrosion offleash Ribs, Skins & Rivets 5 01-04-2008 08:07 PM
galvanic corrosion teemack Ribs, Skins & Rivets 3 07-22-2004 12:22 AM


Featured Campgrounds

Reviews provided by

Disclaimer:

This website is not affiliated with or endorsed by the Airstream, Inc. or any of its affiliates. Airstream is a registered trademark of Airstream Inc. All rights reserved. Airstream trademark used under license to Social Knowledge LLC.



All times are GMT -6. The time now is 09:52 PM.


Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.